Polymer Property : Tensile Strength, Yield = 4575 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.54 MPa
4575 psi
2 in/min; ASTM D638
Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip
COPYLENE™ CH085S is a controlled rheology polypropylene homopolymer resin containing slip additive. COPYLENE™ CH085S is used in injection molding and cast film extrusion applications. Applications..