Polymer Property : Tensile Strength, Yield = 45.87 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.87 MPa
6653 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA S210
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 45.87 MPa
6653 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA S210B
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc.