Polymer Property : Tensile Strength, Yield = 45.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.2 MPa
6560 psi
Type I, 51 mm/min; ASTM D638
PolyOne Maxxam™ PPH-10G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..