Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.1 MPa | 6540 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Dry Blend E6755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | ASTM D638 |
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng.. |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0957 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0510T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9300HF ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SIC 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: High Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9310 ASA, Unreinforced Heat Resistant Heat resistant ASA that is used in the interior/exterior material of automobileInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SRF 2704 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Weather Resistance; Good Impact Resistance; Good Processability Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Te.. |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SRF 1707 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: Good Impact Resistance Uses: Fittings Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron HR-59 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron HR-60 ABS Heat Resistant High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron HI40I ABS Injection Molding Grade Automotive applications -Super High Impact , High Rigidity, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 45.1 MPa | 6540 psi | 9.8 in/min; ASTM D638 |
Teknor Apex Sinvicomp SBB 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Tensile Strength, Yield | 45.1 MPa @Thickness 3.20 mm |
6540 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron IM21G ABS Injection Molding Grade Super High Gloss, Medium ImpactInformation provided by Bhansali |