Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.9 MPa | 6510 psi | 107% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |