Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 44.7 MPa | 6480 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Tensile Strength, Yield | 44.7 MPa | 6480 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |