Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan..
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE..
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer
PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp..