Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.92 MPa
423 psi
AVG Stress at Elongation M25; ASTM D412 Method A
Seals Eastern 7182X Fluorocarbon-Elastomer
Formulated AFLAS®. Ultra-low compressive stress relaxation for alkaline, high-temperature service.Information provided by Seals Eastern, Inc.