Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 248 - 421 MPa | 36000 - 61000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, 1/2 Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |