Polymer Property : Tensile Strength, Yield = 42.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 - 42.7 MPa
4500 - 6200 psi
Average value: 37.3 MPa Grade Count:22
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max..