Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.2 - 42.1 MPa | 2200 - 6100 psi | Average value: 27.4 MPa Grade Count:231 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Tensile Strength, Yield | 19.0 - 42.1 MPa | 2760 - 6110 psi | Average value: 32.8 MPa Grade Count:128 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Yield | 3.38 - 42.1 MPa | 490 - 6110 psi | Average value: 32.7 MPa Grade Count:130 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |