Polymer Property : Tensile Strength, Yield = 4109 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.33 MPa
4109 psi
200°C for 1,000 hrs; ASTM D1458
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..