Polymer Property : Tensile Strength, Yield = 4002 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.59 MPa
4002 psi
ASTM D638
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 27.59 MPa
4002 psi
ASTM D638
Lucent Polymers TPP-240 Polypropylene, 40% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Tensile Strength, Yield 27.59 MPa
4002 psi
ASTM D638
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.