Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.47 MPa | 649 psi | AVG Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 5717 Fluorocarbon-Elastomer FKM. General service.Information provided by Seals Eastern, Inc. |