Polymer Property : Tensile Strength, Yield = 4.137 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.137 - 2571.74 MPa

@Temperature -55.0 - 190 °C
600.0 - 373001 psi

@Temperature -67.0 - 374 °F
Average value: 626 MPa Grade Count:17
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..