Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.75 MPa
399 psi
cured 72 hrs@ RT
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material
QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..