Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.15 MPa | 3938 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 61A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 27.15 MPa | 3938 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 27.15 MPa | 3938 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 61A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 27.15 MPa | 3938 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with Control Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |