Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.50 MPa | 5729 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormod™ HC905TF Polypropylene Homopolymer for Thermoforming Bormod HC905TF is a low melt flow rate polypropylene homopolymer intended for thermoformed packaging applications. This homopolymer is produced using the Borealis Controlled Crystallinity Polypropy.. |