Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.60 MPa | 3858 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 150-1049 HDPE Rotational Molding Resin Description: ICORENEâ„¢ 150-1049 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This prod.. |
|||
Tensile Strength, Yield | 26.60 MPa | 3858 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 150-1498 HDPE Rotational Molding Resin Description: ICORENE 150-1498 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |