Mechanical Properties Metric English Comments
Tensile Strength, Yield 325 - 385 MPa
47100 - 55800 psi
ArcelorMittal HSLA 320 High strength low alloy steel for cold forming, Hot Rolled
Available in the following: S315MCDescription: Steels in the HSLA (High Strength Low Alloy) range are hardened by a combination of precipitation and grain size refining, resulting in high strength w..