Polymer Property : Tensile Strength, Yield = 38.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 38.7 MPa
5610 psi
92% Ret.
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Tensile Strength, Yield 38.7 MPa
5610 psi
300% elongation; ASTM D412; ASTM D638
Lubrizol Estane® 58144 Thermoplastic Polyurethane
Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer..