Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.0 - 38.0 MPa | 2180 - 5510 psi | Average value: 27.4 MPa Grade Count:45 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Tensile Strength, Yield | 22.0 - 38.0 MPa | 3190 - 5510 psi | ASTM D638 |
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Tensile Strength, Yield | 3.50 - 38.0 MPa | 508 - 5510 psi | Average value: 22.1 MPa Grade Count:57 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |