Polymer Property : Tensile Strength, Yield = 3683 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.39 MPa
3683 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 25.39 MPa
3683 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 25.39 MPa
3683 psi
C.O.I.M. PLAXTER® P 52 Polymeric Plasticizer
Description: Formulated with PVC, it is used for the production of insulated cables and stretching films.Information provided by P.A.T. Products, Inc.