Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 363 MPa @Strain 0.200 % |
52600 psi @Strain 0.200 % |
Typical Annealed |
Special Metals INCONEL® C276 Nickel Superalloy Bar Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed bar. Other property values are typical of INCO® C276.Data provided by the manufacturer, Special .. |