Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 36.6 MPa | 5310 psi | |
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Tensile Strength, Yield | 36.6 MPa | 5310 psi | ASTM D638 |
Westlake Plastics Propylux® HS Polypropylene-heat stabilized For Medical Applications Medical grade Propylux HS is made from an FDA approved polypropylene resin. Through a unique heat-stabilizing process, the extruded material is able to withstand higher temperature with less water .. |