Mechanical Properties Metric English Comments
Tensile Strength, Yield 241.4 MPa
35010 psi
ATI Allegheny Ludlum Stainless Steel 334 (UNS S33400)
Allegheny Ludlum Type 334 is a titanium- and aluminum-bearing austenitic stainless steel offering superior elevated temperature scaling resistance compared to the conventional chromium-nickel stainl..