Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.309 MPa | 3380.7 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 150-1119 HDPE Rotational Molding Resin Description: ICORENE 150-1119 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |
|||
Tensile Strength, Yield | 23.309 MPa | 3380.7 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 150-1496 HDPE Rotational Molding Resin Description: ICORENE 150-1496 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is.. |
|||
Tensile Strength, Yield | 23.309 MPa | 3380.7 psi | 2"/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 150-1499 HDPE Rotational Molding Resin Description: ICORENE 150-1499 polyethylene developed for use in rotational molding. It has very high stiffness, toughness, and scratch resistance combined with good processability. This product is .. |