Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 HS L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Tensile Strength, Yield | 228 - 241 MPa | 33000 - 35000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 X 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeighTPCI# 10065101Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Techmer ES HiFill® TPX-HTN-01040 A 45% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Lubrizol ISOPLAST™ 2560 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaAvailableInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Yield | 228 MPa | 33000 psi | ASTM D638 |
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Data provided by Clariant Masterbatches |