Polymer Property : Tensile Strength, Yield = 32600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 - 225 MPa
21000 - 32600 psi
Average value: 186 MPa Grade Count:10
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..