Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 222 MPa | 32200 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific) LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Strength, Yield | 222 MPa | 32200 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON UV00ASU PPA LNP* VERTON* UV00ASU is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: UV Stabilized, Heat Stabilized, Structural. |
|||
Tensile Strength, Yield | 222 MPa @Strain 0.200 %, Temperature 204 °C |
32200 psi @Strain 0.200 %, Temperature 399 °F |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4.. |
|||
Tensile Strength, Yield | 222 MPa | 32200 psi | ISO 527 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA LNP* VERTON* UV00AS is a compound based on Polyphthalamide resin containing 50% Long Glass Fiber. Added features of this material include: Heat Stabilized, Structural. |