Polymer Property : Tensile Strength, Yield = 32.39 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.39 MPa
4698 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 32.39 MPa
4698 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Tensile Strength, Yield 32.39 MPa
4698 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 32.39 MPa
4698 psi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 330ºF Cure Temperature
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..