Polymer Property : Tensile Strength, Yield = 310000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2140 MPa
310000 psi
Typical epoxy composite property
Hexcel® HexTow™ AS2C Carbon Fiber
HexTow™ AS2C carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. This fiber has been surface treated..