Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.00 MPa | 3046 psi | ASTM D638 |
I. Stern 870E High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetprofilesAgency Rating.. |
|||
Tensile Strength, Yield | 21.00 MPa | 3046 psi | ASTM D638 |
I. Stern BLK100 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetProfilesAgency Rating.. |