Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.9 MPa | 3030 psi | 50 mm/min; ASTM D638 |
Phillips Sumika Marlex® CHP-370 Thermoplastic Polyolefin
(discontinued **) Thermoplastic Polyolefin, Good Stiffness and Impact PerformanceApplications: Automotive Pillar TrimConditioning after Molding: 48 hr at 23°CNominal Shrinkage: 0.8-1.0%Drying conditionsTemperature: .. |