Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.04 MPa | 2906 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® DIPP-119 Thermoplastic Polyurethane Elastomer PEARLCOAT® DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this product.. |