Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tensile Strength, Yield | 28.59 MPa | 4147 psi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Hi-Sil 233 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |