Polymer Property : Tensile Strength, Yield = 2784 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.20 MPa
2784 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N990 (MT) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tensile Strength, Yield 19.20 MPa
2784 psi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N990 (MT) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..