Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.13 MPa | 3935 psi | |
C.O.I.M. PLAXTER® P 64 Polymeric Plasticizer Description: Formulated with PVC, it is used for the production of gaskets for refrigerators and other applications.Information provided by P.A.T. Products, Inc. |