Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.00 MPa | 3916 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 91T85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 91T85 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.A.. |
|||
Tensile Strength, Yield | 27.00 MPa | 3916 psi | At 50 mm/min; ISO/DIS 6259 |
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr.. |
|||
Tensile Strength, Yield | 27.00 MPa | 3916 psi | At 50 mm/min; ISO 527-2 |
Borealis Bormod™ BF970MO Polypropylene for Injection Molding Bormod BF970MO is a heterophasic copolymer characterized by an optimum combination of very high stiffness and high impact strength.Bormod BF970MO is a new generation grade for very fast production o.. |