Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.3 MPa | 3810 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 26.3 MPa | 3810 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 350ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 26.3 MPa | 3810 psi | At 50 mm/min; ISO 527-2 |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |