Polymer Property : Tensile Strength, Yield = 258000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1780 MPa
258000 psi
Carpenter AerMet® 100 Aged at 875°F
An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren..