Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.99 MPa | 3770 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91F88 Thermoplastic Polyurethane Elastomer Type: Pearlthane® D91F88 is an aliphatic-based thermoplastic polyurethane.Main Application : ExtrusionSpecial features : Outstanding abrasion loss, excellent color stability upon weather exposure.. |