Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.3 MPa | 3670 psi | 2 in/min; ASTM D638 |
Ineos N00G-01 Polypropylene Impact Copolymer Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa.. |