Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.68 MPa | 243 psi | AVG Stress at Elongation M25; ASTM D412 Method A |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |