Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.38 MPa
2375 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 16.38 MPa
2375 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TCP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 16.38 MPa
2375 psi
ASTM D-638
Axiall 68141 Wire & Cable Flexible PVC
90°C rated, non-lead stabilized compound designed for use as an SE and USE jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 16.38 MPa
2375 psi
ASTM D-638
Axiall 10870 Wire & Cable Flexible PVC
General purpose jacket compound recommended for 60C applications and also suited for 75C at a wall thickness of 30 mils and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp..