Polymer Property : Tensile Strength, Yield = 237 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 237 MPa
34400 psi
5.0 mm/min; ISO 527
PolyOne Nymax™ GF 1200 A 55 HS Natural Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Tensile Strength, Yield 237 MPa
34400 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP QC008 PA6.10
LNP* THERMOCOMP* QC008 is a compound based on Nylon 6/10 containing 40% Carbon Fiber. Added feature of this grade is: Electrically Conductive.