Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.45 MPa | 3401 psi | ASTM D638 |
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 23.45 MPa | 3401 psi | ASTM D638 |
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |