Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.80 MPa
2291 psi
After 14 days, 90°C H<sub>2</sub>O
ACC SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea
EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be ..