Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.58 MPa | >= 229 psi | Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 5717 Fluorocarbon-Elastomer FKM. General service.Information provided by Seals Eastern, Inc. |