Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 226 MPa | 32800 psi | Typical |
Materion AlBeMet® AM 162 HIP'd Billet, Annealed This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) .. |